Subject: | |
From: | |
Reply To: | TechNet E-Mail Forum. |
Date: | Tue, 3 Jul 2001 11:53:32 -0600 |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
I would think you could just calculate the circumference of the via and,
knowing the thickness of the plating in the hole, use the same trace widths
vs. current tables. The trace width is just curled up into a tube. It
should give a close enough approximation for your purposes. If you can fill
the hole with solder, it should be able to handle even more current,
although using reflow usually makes it difficult to keep the solder in the
hole.
-----Original Message-----
From: Malander, Michael [mailto:[log in to unmask]]
Sent: July 3, 2001 11:05 AM
To: [log in to unmask]
Subject: [TN] Via design verses current
I am designing a circuit and I was wondering if there was any standard for
via design verses current like there is for trace widths verses current.
does anyone know a standard like this exists and where I might find
information on it. I have most of the IPC standard documentation on PCB
design but I was only able to find information on blind or hidden vias. Can
I treat a standard via the with the same standard or is there a different
specification for them?
I would appreciate any information on this subject. Thank you for your
help.
Michael Malander
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|