For a good paper see http://www.amp.com/product/articles/dd68_1.html
on the web, Per the Tin Commandments:
"Mating tin-plated contacts to gold-plated contacts is not recommended."
I have this situation on my home computer and sure enuf, after a yaer
I had to re-seat the sims!
Larry Sternig
[log in to unmask]
*** Original Author: ipc.ipc.org!ipc.org! 01/24/96 071745
Resent-Date: Wed, 24 Jan 1996 05:04:36 -0800
Old-Return-Path: <[log in to unmask]>
From: "Terry Davey" <[log in to unmask]>
X-Mailer: Z-Mail (3.0.0 15dec93)
To: [log in to unmask]
Subject: Mating Au-Ni with Sn-Pb connectors
Cc: turnerj@prut
Content-Type: text/plain; charset=us-ascii
Mime-Version: 1.0
Resent-Message-ID: <"MF_-J.0.CdE.UtY1n"@ipc>
Resent-From: [log in to unmask]
X-Mailing-List: <[log in to unmask]> archive/latest/2324
X-Loop: [log in to unmask]
Precedence: list
Resent-Sender: [log in to unmask]
Does anyone out there have experience/knowledge of mating gold-plate edge
contacts (on SIMMS - so dry contacts) with tinned connectors. Is it a no-no
from a long-term reliability point of view?
We have a first source with tinned edge contacts (matching the connector) and
are lokking at a gold-plate second source.
Terry Davey [log in to unmask]
|
|
|