Jan,Stella, and other technetters,

        My apologies for the error-I just got the alloys switched, thanks guys
for catching the error. Bronze= Copper/Tin alloy & Brass=Copper/zinc alloy. We
dont need errors of this kind floating around.


Regards,

Les Connally