You need to go with a tolerance of .008 dtp. Most of the vendors
should be able to build the boards with this number. .006 is
especially tight for large quantities. You should also ask your
vendor to provide you with a capability study of there drill
operation. If your supplier has one and if the sample size is
considerably large then you will see that .008 dtp is the way to go.
______________________________ Reply Separator _________________________________
Subject: Re: [TN] PTH Positional Hole Tolerance
Author: "TechNet E-Mail Forum." <[log in to unmask]>, at corp
Date: 3/13/98 6:04 AM
We used to spec the same tolerance. Never heard a peep of complaint from
most fab houses, the only one who complained was known by engineering to do
a poor job generally (but loved by our tight-fisted purchasing agent).
Jay DeKing
EMA Mid-Atlantic, Inc.
(716)334-2970 voice
(716)334-3481 fax
[log in to unmask]
-----Original Message-----
From: Richard G Smith [SMTP:[log in to unmask]]
Sent: Friday, March 13, 1998 8:26 AM
To: [log in to unmask]
Subject: [TN] PTH Positional Hole Tolerance
Hi All,
Here's the issue:
We specify in our fab spec that all holes are to be within .003" of
their corresponding pad center (true position of .006"). We are being
told by our fab house that this tolerance is unreasonably tight.
Any comments???
Thanks,
Rick
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|