Here's another what we do:
As a rule any hole beneath .030" is used as a via, and therefore not
soldered to.
We the add to our drill table the following:
1. Holes smaller than 30 mils show nominal finished size, but no
tolerance.
2. Added column shows drill size (nominal +.005") +/-.001 (allows 2-3
drill availability) for any hole without tolerance.
3. Add a note stating - HOLES WITH DEFINED DRILL SIZES MAY BE PLATED
SMALLER THAN NOMINAL.
This allows us to define outer barrel diameter, follow our stated
minimum .001" hole wall thickness, and compensate for plating variance
between small holes (<.030") and large holes (>.100").
Our suppliers seem to be very comfortable with this, giving us high
yields and we don't have hole issues at assembly.
Just another way to achieve the need.
FNK
Frank N Kimmey CID+
Principal PCB Designer
PCB Programs
Powerwave Technologies Inc
Office 916-941-3159
Fax 916-941-3195
Mobile 916-670-0645
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Karl Hunsinger
Sent: Friday, April 27, 2007 11:42 AM
To: [log in to unmask]
Subject: Re: [TN] "plated shut vias"
Our drawings almost always have a tolerance associated for vias. As
Ramon just stated, we add a "plating factor" to the specified hole size
to obtain the drill size. The expectation is to finish at the nominal
(middle of the tolerance) hole size.
Karl
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Dehoyos, Ramon
Sent: Friday, April 27, 2007 2:32 PM
To: [log in to unmask]
Subject: Re: [TN] "plated shut vias"
Agreed, We just went through such an exercise and the conclusion
was that the specified hole size was the final hole size. A 6, 7, 8 or 5
mils were added to find the drill size.
Ramon
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Smith, Richard
Sent: Friday, April 27, 2007 10:05 AM
To: [log in to unmask]
Subject: Re: [TN] "plated shut vias"
I don't disagree but, unless I'm behind the times which is entirely
possible, the IPC used to promote the practice of specifying all plated
hole sizes as finished permitting the manufacturer to select the
appropriate drill. I'm not implying this is the best practice, but on
the other hand I've not seen a via reliability issue attributable to the
finished via hole tolerance on the drawing.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Werner Engelmaier
Sent: Thursday, April 26, 2007 3:23 PM
To: [log in to unmask]
Subject: Re: [TN] "plated shut vias"
Hi All,
Vias should never be specified in terms of finished hole size (there is
no
functional need for any specific finished hole diameter), but in terms
of
drilled hile diameter, because that determines all kinds of things
important to the reliability of the via interconnect structure.
Werner
**************************************
See what's free at http://www.aol.com.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|