Hello guys , I need some assistance in the ink preparation
for the LPSM .Currently I am using Peter's ink and really
interested to know what should be the correct rpm for
the ink preparation and for how long the stirring should be .
I have encountered soldermask bubbles defect . Do temperature
in the room affects the bubbling so much although I do
understand low
temperature do help in reducing the bubbling .
Please advise .
Thanks.