Ed ,
not everybody is so lucky to be able to stick with HASL .
We all don't particularly crave on the "glamour" of the solderability of
the alternative finishes ; because there is none .
The complexity of the design usually forces you to fairly desperate
solutions as NiAu is just one example .
If you have to assemble, switch, contact, not oxidize (as some), stay
level (helps) ; all on one board ; you have little choice ; but try
harder .
Crack your mobile open and start the education .
Besides that , you are quite right , HASL is expensive, poisonous, hot,
energy hungry, dangerous, bumpy process .
We all love HASL as much as you do . But ..........
If you do straight solder only , try the new AlphaLevel , it solders
almost as well .
See you paul
>----------
>From: Eddie Brunker[SMTP:[log in to unmask]]
>Sent: Friday, 17 April 1998 21:40
>To: [log in to unmask]
>Subject: Re: [TN] CALL FOR PAPERS: IPC 1998 Surface Finishes Conference
>
>At 21:46 16/04/98 -0500, you wrote:
>>
>>
>>
>>
>>Hi TechNet -
>>
> HASL finishes are quite
>>robust in many assembly operations but can be equally non-robust in other
>>assembly operations.
>
>It would be useful to have a discussion on the specific situations where
>this is the case.
>
>
>In addition there are a number of IPC committees (e.g.
>>ANSIJ-STD-002/003, and the Alternative Solderable Finishes task group) that
>>have an active interest in the latest developments in the alternative
>>finishes activities.
>
>I agree that we must look to the future. But why look for complex answers
>when simple ones already exist.
>
>As stated earlier, education may hold the key, but that's not as exciting or
>glamorous as a new PCB finish.
>
>
>>
>>Dave Hillman
>>Rockwell Collins
>>[log in to unmask]
>>
>>
>
>P.S. Again, please excuse any illmannered ranting and raving on my part
>earlier.
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
>information.
>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
>847-509-9700 ext.311
>################################################################
>
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|