TECHNET Archives

1996

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
[log in to unmask] (Chris Hunt, National Physical Laboratory)
Date:
Mon, 1 Jul 1996 18:03 BST
Content-Type:
text/plain
Parts/Attachments:
text/plain (21 lines)
The IEC has just completed a wetting balance test for SM components, IEC
68-2-69, using the solder bath and the solder globule. It is currently
working on a wetting balance test for printed circuit boards. It has
carried out one intercomparison and is planning a second.


Chris Hunt
National Physical Laboratory
Centre for Materials Measurement Technology
Building 15
Queens Road
Teddington
Middlesex
United Kingdom TW11 0LW

Tel +44 (0) 181-943 7027 direct or switchboard 0181-977 3222 ext 7027 
Fax: +44 (0)181-943 6453
E-mail:     [log in to unmask]