Looks like plating defect to me- I would contact your board supplier.
Brien Bush
Manufacturing Applications Specialist
Cirtronics corp.
Milford, N.H.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Wednesday, July 30, 2014 8:02 AM
To: [log in to unmask]
Subject: [TN] Spots on Gold
Morning John,
I have your second photo posted, it's here:
http://stevezeva.homestead.com/ring.jpg
This looks interesting!
Steve
On Tue, Jul 29, 2014 at 5:56 PM, <[log in to unmask]> wrote:
> Hi steve
>
> I managed to get to a good microscope this afternoon. Everyone of
> these spots looks like someone circled it* w*ith a magic marker.
>
> Would you mind posting one more pic for me.
>
> Thanks
>
> John Foster
>
>
>
--
This email and any attachments are only for use by the intended
recipient(s) and may contain legally privileged, confidential, proprietary or otherwise private information. Any unauthorized use, reproduction, dissemination, distribution or other disclosure of the contents of this e-mail or its attachments is strictly prohibited. If you have received this email in error, please notify the sender immediately and delete the original.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
WARNING: Export Control This message, including any attachments, may contain technical data within the definition of the International Traffic in Arms Regulations (ITAR), and subject to the Export Control Laws of the U.S. Government. Transfer of such information by any means to a foreign person, whether in the United States or abroad, without proper export authorization or other approval from the U.S. Department of State is prohibited.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|