We have had good results with only 1 sheet of prepreg. Be cautious the
lamination press, tooling and all have to be in better shape as you loose
much of the tendency to level out unevenness. You will se this as voids in
the material amo.
Use prepregs with high resin content.
Good luck !
Jan
-----Oprindelig meddelelse-----
Fra: Malewicz Wesley [mailto:[log in to unmask]]
Sendt: 15. marts 2002 00:32
Til: [log in to unmask]
Emne: [TN] Prepreg
What are the Pro and Con's of using a single sheet of prepreg vers using two
sheets of prepreg? In our fabrication specification we specify that we
require that two sheets of prepreg are to be used. For as long as I can
remember we have always had this requirement and I would like to have a
better understanding as to why we might need to continue.
Thanking you in advance for your response.
Wes
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|