Hi Mike,

Even though we are not in the are but deal with that kind of problems on a daily base and our customers from the are have no problem sending samples for analysis over.

You can contact me of line if you wish.
Vladimir

SENTEC Testing Laboratory Inc.
11 Canadian Road, Unit 7.
Scarborough, ON M1R 5G1
Tel: (416) 899-1882
Fax: (905) 882-8812
www.sentec.ca

-----Original Message-----
From: "[log in to unmask]" <[log in to unmask]>
Sender: TechNet <[log in to unmask]>
Date: Fri, 23 Sep 2011 16:56:30 
To: <[log in to unmask]>
Reply-To: "[log in to unmask]" <[log in to unmask]>
Subject: [TN] tiny cracks in solder

I'm looking for help solving a quality/reliabilty problem with cracked solder on fine pitch SMT  solder joints.    Have not been able to completely eliminate the condition and from time to time see downstream failures that exhibit the cracked solder condition.   Our own process experts are ready to find an outside consultant that can guide us to health.  What's the best way to find an effective expert  in the LA area that we might hire to consult with.  
 
Mark Julstrom

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________




---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 16.0

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815

-----------------------------------------------------


ATOM RSS1 RSS2