Leland,
I have trouble remembering my drive to work, so I can relate! Even though the doc was for SMT, I thought you might be referring to this one.
Regards,
Sue
From: Leland Woodall [mailto:[log in to unmask]]
Sent: Wednesday, August 24, 2011 12:17 PM
To: James, Susan CAR; [log in to unmask]; [log in to unmask]; [log in to unmask]
Subject: RE: Wave Soldering Process Fishbone Diagram
Susan,
That’s the document to which I referred. Gee, I didn’t realize it had been that long ago. No wonder I couldn’t locate it.
I was mistaken though about the process. Thought it was aimed at the wave and not SMT. Guess my seven year memory capability is not what I’d perceived it to be!
Leland
From: James, Susan CAR [mailto:[log in to unmask]]
Sent: Wednesday, August 24, 2011 1:02 PM
To: [log in to unmask]; Leland Woodall; [log in to unmask]; [log in to unmask]
Subject: Re: Wave Soldering Process Fishbone Diagram
Here’s a copy of a fishbone I saved from Inge from “way back” to 2004. Actual diagram is on page 4. If this is the one you’re looking for, I’ve sent a copy to Steve to post if he wants to.
Regards,
Sue
Susan James
Engineer, Taylor Company
a division of Carrier Commercial Refrigeration, Inc.
United Technologies Corporation
Date: Wed, 24 Aug 2011 08:17:55 -0400
From: Steve Gregory <[log in to unmask]>
Subject: Re: Wave Soldering Process Fishbone Diagram
Hi Leland,
I'm sorry that I didn't respond sooner, I got busy and forgot about your email. I sincerely apologize.
I looked for the fishbone that Inge sent, and I couldn't find it. I must have taken it down from my web page when I cleaned it up some months back. But as I recall, I don't think it was specifically for wave soldering. Maybe if Inge has his ears up, he can resend it and I'll post it again on my page.
But what I did find is a good reflow/wave problem & trouble-shooting chart put out by Electrovert. I don't know if you've seen it before. I'll send it along with this email...
Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Leland Woodall
Sent: Wednesday, August 24, 2011 6:37 AM
To: [log in to unmask]
Subject: [TN] Wave Soldering Process Fishbone Diagram
Folks,
A few months ago I remember a fellow TechNetter making available to the group a fishbone diagram of the wave soldering process. I'm usually pretty good about hanging onto stuff like this, but have apparently misplaced this one. If someone has a copy, could you please forward me a copy?
By the way, Clumpy and his cousin were both helping out quite well until about 2:00 yesterday. I think the aftershocks of the earthquake kinda shook them up, and they asked for the remainder of the day off.
Leland
________________________________
“Confidentiality Notice:
This transmission (including any attachments) may contain confidential information belonging to the sender and is intended only for the use of the party or entity to which it is addressed. If you are not the intended recipient, you are hereby notified that any disclosure, copying, distribution, retention or the taking of action in reliance on the contents of this transmission is strictly prohibited. If you have received this transmission in error, please immediately notify the sender and erase all information and attachments.”
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|