Hi All
We just had a customer raise a concern regarding some SMT connectors. What
they noticed was the solder tails all being raised in the solder. Not 1
lead on any connector was flat to the pad.
What we noticed was the solder tails are not on the same plane as the
fitting nails of the connectors. When you place the connector flat to the
PCB, the solder nails are off the pad by about 0.005", which can cause a
problem when you have a 0.006" stencil.
I have contacted the manufacture but have yet to hear anything.
Has anyone run across this concern before? Any info would be appreciated
Thanks
Andre
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------