Item Subject: [TN] Optically transparent epoxy
Mark,
Is the material used for casting on PCB board? You can try Dexter and
Pacific Technology. All these kind of material are high moisture
sensitivity and very high CTE. The mismatch of CTE among packaging
material can cause delamination and wire break. You must fully
understand the interaction of design and material properties. It is
suggested the design and material selection should guided by FEM
analysis.
What is your application?
Eden
______________________________ Reply Separator _________________________________
Subject: [TN] Optically transparent epoxy
Author: Non-HP-Mark Elliott ("Mark Elliott"@maxtek.com) at
HP-Singapore,shargw51
Date: 8/12/98 4:20 AM
Technetters,
I am looking for an optically transparent epoxies for use as a potting
compound that can withstand IR reflow. This epoxy must be very stable and not
absorb moisture. Also air bubble must be kept to a minimum. Recommendation
on manufacturers, suppliers, or specific products would be much appreciated.
Also any information on reliability of these products would be also help.
Thanks for your help,
J. Mark Elliott
Maxtek Components Corp.
503.627.3641
[log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for
additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700
ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|