Subject: | |
From: | |
Date: | 06 Jun 1996 12:02:41 -0500 |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
I think this may be an old address:
Plating is the magazine of the AESF which used to be the AES
I believe the current address is:
American Elecroplaters and Surface Finishing Society
12644 Research Parkway
Orlando FL 32826
407-281-6441
FAX 407-281-6446
----------
From: [log in to unmask]
To: [log in to unmask]
Subject: Gold Plating Specs and other information
Date: Wednesday, June 05, 1996 2:39PM
Contact: American Electroplaters' Society, Inc
56 Melmore Gardens
East Orange, New Jersey 07017
Also look in the journal 'Plating' which has ton of information on plating
related issues. There is a good paper on Gold Plate Spec for electronics
equipment by RG Baker and TA Palumbo, Plating, August 1971, pp 791-800.
|
|
|