Ben,
Yes, from our results components were non planar post soldering and
touch up of open circuits nigh on impossible, requiring a full rework,
i.e. removal & replacement. The next iteration of the board with these
components on is on the horizon, I was wondering if anyone had working
footprints/stencil designs?
Regards,
Iain
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gumpert, Ben
Sent: 13 October 2011 13:07
To: [log in to unmask]
Subject: Re: [TN] [DC] QFN layout
Iain,
Do you mean soldering? Yes, very tricky. The pulled-back terminations
make it very difficult to tell if a good joint has been made. And that's
a lot of gold. Gold removal can make the issues even worse.
Ben
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Braddock, Iain (UK)
Sent: Thursday, October 13, 2011 7:11 AM
To: [log in to unmask]
Subject: EXTERNAL: Re: [TN] [DC] QFN layout
Anyone successfully processing QFN components like Hittite's HMC553LC3B,
especially with a Mydata........tricky little rascal?
Regards,
Iain
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bush, Brien
Sent: 13 October 2011 11:38
To: [log in to unmask]
Subject: Re: [TN] [DC] QFN layout
*** WARNING ***
This mail has originated outside your organization, either from an
external partner or the Global Internet.
Keep this in mind if you answer this message.
Hi Paul,
We have been using Mydata's for the past 20 years. We also place QFN'S
and LGA's. We have had our share of Issues, but we are able to process
these parts very well now. We can tell the machine where to test the
board Level and use no place force. When these parts are place, you will
not see any board deflection.
I find the Mydata machines very user friendly.
Brien Bush
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Tan Geok Ang
Sent: Thursday, October 13, 2011 3:34 AM
To: [log in to unmask]
Subject: Re: [TN] [DC] QFN layout
Hi Paul,
Like your statement "we don't use MyDatas for QFNs"
should add and "LGA".
Really hope that MyData able to solve this issue which I
believe through their software control with Z-height head/Component
thickness/Board flat measurement information, etc.
Regards
Geok Ang
(Office: 68712393)
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Paul Edwards
Sent: Wednesday, 12 October 2011 8:22 AM
To: [log in to unmask]
Subject: Re: [TN] [DC] QFN layout
Bob,
It would be if I told you that we released the part after we deformed
the solder paste 30%...
And that's why we don't use MyDatas for QFNs...
Paul
Paul Edwards
Process/Quality Engineering
Surface Art Engineering
-----Original Message-----
From: Robert Kondner [mailto:[log in to unmask]]
Sent: Tuesday, October 11, 2011 11:59 AM
To: 'TechNet E-Mail Forum'; Paul Edwards
Subject: RE: [TN] [DC] QFN layout
Paul,
Hmmmm so you say you don't deform the solder paste thickness by more
than 30%. Hmmm.
Since the paste is probably about 4 or 5 mils high that means you
position the part within about 1.5 mils. Hmmmm
Considering the PCB thicknesses vary more than that, and part
thicknesses vary more than that, and board flatness is much further off
than 1.5mil ...
I would suggest your comment is pure hog wash? :-)
Bob K.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Paul Edwards
Sent: Tuesday, October 11, 2011 12:46 PM
To: [log in to unmask]
Subject: Re: [TN] [DC] QFN layout
Bob,
We measure the part and PCB warp and vary the part vacuum release point
based on that to insure we are not deforming the printed solder paste
structure more than about 30%...
Because the MyData can't do that we don't typically use the MyData for
QFNs...
Paul
Paul Edwards
Process/Quality Engineering
Surface Art Engineering
-----Original Message-----
From: Robert Kondner [mailto:[log in to unmask]]
Sent: Tuesday, October 11, 2011 9:49 AM
To: 'TechNet E-Mail Forum'; Paul Edwards
Subject: RE: [TN] [DC] QFN layout
Paul,
I don't think we are on the same wavelength.
Are you telling me you can drop a part 50mil onto a board to avoid
pressing it down into the paste? I cannot imagine doing that and getting
any placement accuracy. That would be nonsense.
It is in the force sensor where the machine detects board contact.
Also,
watch the board deflection as a part is placed, you would be surprised.
The
MyData's allowed me to slow down placement to where you can actually see
this deflection.
Bob K.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Paul Edwards
Sent: Tuesday, October 11, 2011 12:09 PM
To: [log in to unmask]
Subject: Re: [TN] [DC] QFN layout
Normally we set the machines to a height placement point for QFNs to fix
the problem BUT you can do that on all machines and in ALL cases but
when you can it eliminates most of the problems...
Paul
Paul Edwards
Process/Quality Engineering
Surface Art Engineering
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Robert Kondner
Sent: Tuesday, October 11, 2011 8:51 AM
To: [log in to unmask]
Subject: Re: [TN] [DC] QFN layout
Karen,
Sadly I know more about the problems and not as much about the
solutions!
:-(
For example the placement force on most Pick and Place (PnP) machine
has a minimum setting. If you place a small part with a small number of
leads the "Pressure" (Force / Area) on the paste is very high and can
squish paste into places you don't want it.
Take a look at a board as if comes off a PnP machine. Lift of some
small parts and you will see that leads have been pushed down through
the paste to the PCB copper. This works great for gull wing parts, it
helps insure a good reflow. But guess what happens on a small QFN?
Actually the paste on the large center thermal pad helps act like a
standoff.
But, how flat is the PCB as it sits on the PnP and where did the
operator decide to place board supports? So much for the part coming
down flat onto the PCB as it is placed!
Ugh, so many problems and so few solutions!
Bob K.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Karen Tellefsen
Sent: Tuesday, October 11, 2011 10:39 AM
To: [log in to unmask]
Subject: Re: [TN] [DC] QFN layout
How does one do these calculations, what are the rules?
Is there a web site that can provide guidance? QFN's are difficult to
solder well
Karen Tellefsen - Electrical Testing
[log in to unmask]
908-791-3069
Re: [TN] [DC] QFN layout
Robert Kondner
to:
TechNet
10/11/2011 10:29
AM
Sent by:
TechNet <[log in to unmask]>
Please respond to rkondner
Pete,
I agree. Sometime it is less of an agenda and more of a case of never
having reflowed these parts.
My observation with QFNs has suggested having a good .5 to 1.0 mm of
pad outside the package. It acts like a solder reservoir area allowing
solder to flow out from under the leads as the component reflows and
settles down.
So often I see suggest QFN footprint with no such area.
Just a non-qualified observation.
Bob K.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Pete
Sent: Tuesday, October 11, 2011 9:32 AM
To: [log in to unmask]
Subject: Re: [TN] [DC] QFN layout
I never trust the manufacturer's suggested footprint, always do my own
calculations. They have a different agenda than I need to have.
Lately,
though, I'm finding their footprints much closer to mine.
Pete
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives For
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100
ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives For
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100
ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives For
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100
ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives For
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100
ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives For
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100
ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives For
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
WARNING: Export Control
This message, including any attachments, may contain technical data
within the definition of the International Traffic in Arms Regulations
(ITAR), and subject to the Export Control Laws of the U.S. Government.
Transfer of such information by any means to a foreign person, whether
in the United States or abroad, without proper export authorization or
other approval from the U.S. Department of State is prohibited.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives For
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
********************************************************************
This email and any attachments are confidential to the intended
recipient and may also be privileged. If you are not the intended
recipient please delete it from your system and notify the sender. You
should not copy it or use it for any purpose nor disclose or distribute
its contents to any other person.
MBDA UK Limited, a company registered in England and Wales, registration
number 3144919 whose registered office is at Six Hills Way, Stevenage,
Hertfordshire, SG1 2DA, England.
********************************************************************
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives For
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives For
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|