Hi Brien,
I run closed-loop here, and we use Bivar dissopads. I was worried about
using them, but so far it doesn't seem as bad as I thought. In the six
months that I've been here, we've changed the resin beds once. I've got
two carbon beds in front of a cation, anion, and mixed bed. We also use
Techspray Wondermask WSOL, which I was also worried about, but doesn't
seem as bad as I thought as well. I get a little pink residue inside the
washer tank, but so far it removes fairly easy. We have a Austin America
Microjet EC cleaner.
I got a sample of spacers from Multi-Seal that I'm going to be trying.
Check out:
http://www.multi-seals.com/washawayspacers.php
Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bush, Brien
Sent: Thursday, October 17, 2013 6:41 AM
To: [log in to unmask]
Subject: Re: [TN] Charred dissopad residue
Hi Ed,
I was just curious to see if you are using DI closed loop wash system.
We had to stay away from the wash away spacers because they Were causing
problems with our mixed resin beds. Have you had any issues?
Regards,
Brien
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bob Landman
Sent: Thursday, October 10, 2013 5:36 PM
To: [log in to unmask]
Subject: Re: [TN] Charred dissopad residue
Maybe your boards are lactose intolerant?
Do you have to go lead-free? Thankfully we do not.
Bob
Sent from my iPhone
On Oct 10, 2013, at 5:21 PM, Ed Popielarski <[log in to unmask]>
wrote:
> Bivar uses lactose and sodium chloride. So now the question is "should
we cry over burnt milk"?
>
> Ed Popielarski
> Engineering Manager
>
>
> 970 NE 21st Ct.
> Oak Harbor, Wa. 98277
>
> Ph: 360-675-1322
> Fx: 206-624-0965
> Cl: 949-581-6601
>
> https://maps.google.com/maps/myplaces?hl=en&ll=48.315753,-122.643578&s
> pn=0.011188,0.033023&ctz=420&t=m&z=16&iwloc=A
>
>
> -----Original Message-----
> From: Steve Gregory [mailto:[log in to unmask]]
> Sent: Thursday, October 10, 2013 2:19 PM
> To: [log in to unmask]; Ed Popielarski
> Subject: RE: [TN] Charred dissopad residue
>
> Hey Ed,
>
> Haven't run across that problem (yet), and don't really know how to
clean that. But I did run across another brand of spacers that I didn't
know about before that's made of different material than what Bivar
dissolvable spacers are made of...aren't bivar spacers made of some sort
of sugar ?
>
> http://www.multi-seals.com/washawayspacers.php
>
> They're made of something called Polyvinylpyrrolidone, and contain no
ionizable material, salts, sugars, metals, or soaps, and they are
non-corrosive, non-conductive, and non-toxic.
>
> I just found them in a search today. I'm getting a sample pack of them
sent to me check them out myself, you might check them out too if you've
never tried them.
>
> Steve
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Ed Popielarski
> Sent: Thursday, October 10, 2013 2:31 PM
> To: [log in to unmask]
> Subject: [TN] Charred dissopad residue
>
> Hi all,
>
> Had an odd problem today.
>
> We have built many of these assemblies with tin/lead solder but just
now switched to lead free solder (higher temperature).
>
> The "Dissopad" contacting the PCB (at a via) liquefied, spread and
> charred. The residue is very difficult to remove, especially a concern
> since it is under components and could be "conductive". (pix available
> on request)
>
> We tried cleaning this with isopropyl alcohol and it didn't seem to
dissolve the charred residue at all.
>
> I soaked one PCB in 140F DI water for 30 min. and re-cleaned in the
aqueous cleaner. It did seem to remove the heavier residue, but there
remains a film and smaller clumps on the board surface.
>
> Any suggestions would be appreciated!
>
>
> Ed Popielarski
> Engineering Manager
>
> [Description: FullLogo]
> 970 NE 21st Ct.
> Oak Harbor, Wa. 98277
>
> Ph: 360-675-1322
> Fx: 206-624-0965
> Cl: 949-581-6601
>
> https://maps.google.com/maps/myplaces?hl=en&ll=48.315753,-122.643578&s
> pn =0.011188,0.033023&ctz=420&t=m&z=16&iwloc=A
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud
service.
> For more information please contact helpdesk at x2960 or
> [log in to unmask]
> ______________________________________________________________________
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud
service.
> For more information please contact helpdesk at x2960 or
> [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
WARNING: Export Control
This message, including any attachments, may contain technical data
within the definition of the International Traffic in Arms Regulations
(ITAR), and subject to the Export Control Laws of the U.S. Government.
Transfer of such information by any means to a foreign person, whether
in the United States or abroad, without proper export authorization or
other approval from the U.S. Department of State is prohibited.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|