Hello Technetters:
Processing a 16"x20", .125" thick double-side mixed-tech (smt both sides,
and pth component side) with at least two .8mm BGAs with .45mm balls:
one is a 84 pin package is a 9 x 15 - 135 - ball matrix with 51
depopulated balls in the center of the package
the other is a 8 x 12 - 96 ball - matrix with 8 depopulated balls - 4 at
either end of the matrix
Two quick questions:
Can I clean (in-line) using di water only if I use OA flux? Or, do I need
to switch to no-clean for BGAs less than 1mm?
For rework, flux only? Or can I micro-stencil or dispense?
As always, thanks in advance for your replies,
Al Kreplick
Sr. Mfg. Eng.
Teradyne, Inc.
500 Riverpark Drive
Mail Stop NR500 1-1
North Reading, MA 01864
Tel: 978-370-1726
Pager: 888-561-6485
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
PS: Go Red Sox!
|
|
|