For the magnetic wire we have used in the past this has worked well:
Insulstrip Jell
Ambion Corporation
37 Naugatuck Drive
Naugatuck, CT 06770
(203) 723-1437
>Looking for a recommendation for a chemical stripper to strip bi-filar (?)
>magnet wire. Any suggestions?
>
>Jim Marsico
>Senior Engineer
>Production Engineering
>EDO Electronics Systems Group
>[log in to unmask] <mailto:[log in to unmask]>
>631-595-5879
>
>---------------------------------------------------------------------
>------------
>Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt delivery of Technet send the following message:
>SET Technet NOMAIL
>Search previous postings at: www.ipc.org > On-Line Resources &
>Databases > E-mail Archives
>Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
>information, or contact Keach Sasamori at [log in to unmask] or
>847-509-9700 ext.5315
>---------------------------------------------------------------------
>------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------