Gabriela,
You can't use SERA as set up with the borate buffer, but with a
different buffer, and I think in a circulating mode, you can do what you
are asking. The technique is called PESO. Contact Dave Hillman at
Rockwell Collins 319-295-1615 or Peter Bratin at ECI, who make the SERA
tester. They can give you the details.
regards,
Bev Christian
Nortel
>----------
>From: Gabriela Bogdan[SMTP:[log in to unmask]]
>Sent: Wednesday, March 11, 1998 6:06 PM
>To: [log in to unmask]
>Subject: [TN] Contact resistance
>
>Dear Technetters!
>We experience high contact resistance on keyboards.
>The plating is 0.15u Au on 6u Ni.
>1.Could I use SERA in order to see if there is a contamination on the
>keypads
>in comparison to the bare boards?
>2.If YES, HOW?
>3.How could I compare the porosity of the gold plating of two different
>batches ?
>Thank you in advance
>Gaby
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
>text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
>information.
>For the technical support contact Dmitriy Sklyar at [log in to unmask] or
>847-509-9700 ext.311
>################################################################
>
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|