No experience yet, but we have ordered one. Should know something in a
few weeks, if we don't
get too sidetracked in moving everything to a new building.
Charlie Barker
Input/Output, Inc.
713/276-3328
[log in to unmask]
To: TechNet @ ipc.org
cc: (bcc: Charles Barker/IO-US)
From: TechNet @ ipc.org
Date: 08/13/96 09:29:34 AM MST
Subject: SOLDER WAVE OPTIMIZER
We are investigating the Solder Wave Optimizer made by
Technology Information Incorporated. Do any of you
co-TechNetters have any experience with this tool? What are
the pros and cons of the tool? Your comments would be
welcome. Thanks in advance.
Ron H.