Hi Steve! Collins has been down that road a couple of times and while it
may seem like a reasonable, simple method of cleaning assemblies the
problem is that the majority of commercial dishwashers can not withstand
the rigors of DI water and/or other typical cleaning chemistries. What
seemed like an initial success quickly turned into a dishwasher turning
itself into a pile of parts with the assemblies becoming dirtier than they
were before cleaning. I recommend against trying to use a commercial
dishwasher and investigate something in a more industrial mode. Good Luck.
Dave Hillman
Rockwell Collins
[log in to unmask]
Steve Gregory <[log in to unmask]>@ipc.org> on 07/09/2002 08:08:17 PM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
to [log in to unmask]
Sent by: TechNet <[log in to unmask]>
To: [log in to unmask]
cc:
Subject: [TN] Water soluble batch washers...
Hi all,
This is a little bit off-the-wall, and maybe sounds a bit cheap, but I'm
going to ask anyway...
We have a inline water soluble cleaner (an Electrovert H-500) that is
located
at one end of the plant. Problem is, that at the other end of the plant
there
is hand soldering (rework and touch-up) being done. As probably many of you
have learned, operators don't want to make the trip all the way down to the
other end of the plant to get their boards cleaned until they have a rack
of
boards that will make the trip worthwhile... which is understandable from a
purely logistics point of view. But that sometimes results in the flux
residues being left on the boards longer than what is desired.
So the idea was brought up to get a couple of small batch cleaners closer
to
the area so that it would be so much of a trek to get the boards cleaned in
a
timely manner.
Sounds like a good idea. My question is, most of the batch cleaners I've
seen
are glorified dishwashers. When you price these units you find that they
are
much, much more expensive than a dishwasher, but the operating systems are
basically the same. I did a search for commercial dishwashers and can find
nice beefy stainless constructed ones that have heated wash and rinse
cycles,
decent powered pumps, that are a third of the price that some of
"specifically designed for printed circuit cleaning" washers cost.
The wash nozzles are basically the same, rotating wands. Rack systems are
the
same, roll-in, roll-out racks that look very similar to what I've seen in
every dishwasher I've ever had in my home.
So my question is, has anybody ever had a real dishwasher in use to clean
water soluble residues? We will supply DI water to them straight from the
resin beds, and will be able to set appropiate cycle times to ensure
thorough
cleaning.
From my take on things, this should work pretty good without having to
spend
a bunch of money on a machine that can be had for much cheaper and not
actually called "A printed circuit assembly batch aqueous cleaner"...
Any comments?
-Steve Gregory-
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|