GETEK is made by General Electric's "GE Electromaterials" division.
Overview of GE Electromaterials is on WWW at
http://www.ge.com/electromaterials/pe2.htm
Joe Vendetti, Market Development Specialist with GE Electromaterials can be
reached at 401-245-8002 or
e-mailed at [log in to unmask] GE also has a
toll-free product information phone number: 1-800-848-3710.
The GETEK resin system is an epoxy/PPO blend (PPO is polyphenylene oxide).
At 01:25 PM 6/4/96 PST, Sherman Banks wrote:
>
>
>
>I am interested in getting technical data on a PWB material called
>"Getek" Can anyone please tell me the manufacturer and, if possible give
>me contact information?
>
>Thanks in advance
>
>
>
>
David Estes
PCB Commodity Management
Texas Instruments
ph: 214-997-2942
fax: 214-997-2656
e-mail: [log in to unmask] (or the above address)
|
|
|