2nd attempt to be heard. I have done entry work to be in, but got a
fault message from somewhere. Once again...Question: We have bought
subminiature coax connectors for SMT. They have
2um Gold over Brass (body) without Nickel barrier. I don't like the risk
of Zn-leakage. Am I too oldfashioned? People put Tin directly on Kovar
terminals etc. As I cannot handle roller blades, and have spent many
years in a Quality Lab, I may be after my time....../Ingemar /EMW
***************************************************************************