Both of the major players (Buehler or Struers) will do.
Regards,
Vladimir
SENTEC
Sent from my BlackBerry 10 smartphone on the Rogers network.
Original Message
From: Lehmicke, Michael
Sent: Wednesday, December 14, 2016 00:52
To: [log in to unmask]
Reply To: TechNet E-Mail Forum
Subject: [TN] Grinders/polishers for x-sections
This may generate a lively discussion.
What is the best Auto Grinding/Polishing system for high volumes of x-sections?
Thanks,
Mike
Mike Lehmicke
Project Engineer
DSS Division
Molex, LLC-Printed Circuit Solutions
22 Empire Drive
St. Paul, MN 55103
651-846-7728
[log in to unmask]<mailto:[log in to unmask]>
[cid:[log in to unmask]][cid:[log in to unmask]]<http://www.molex.com/>
________________________________
CONFIDENTIALITY NOTICE: This message (including any attachments) may contain Molex confidential information, protected by law. If this message is confidential, forwarding it to individuals, other than those with a need to know, without the permission of the sender, is prohibited.
This message is also intended for a specific individual. If you are not the intended recipient, you should delete this message and are hereby notified that any disclosure, copying, or distribution of this message or taking of any action based upon it, is strictly prohibited.
English | Chinese | Japanese
www.molex.com/confidentiality.html
|
|
|