Regarding the IPC-TM-650 test procedure for No-Flow prepreg (#2.3.17.2), I have a question. In the text, it states to punch two 25.4mm (1in) diameter holes approximately in the middle of the specimen, and refers to figure #1. In figure #1 it shows two 15.9mm (0.625 in) diameter holes. Can you please clarify?