TECHNET Archives

May 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Graszl, Gerry (FL51)" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Tue, 5 May 1998 13:54:08 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (62 lines)
MEK will dissolve alot of plastics but I don't know if it still can be
purchased/used.  I found Dynaloy in a vender cat list ...see below

Dynaloy inc
7 Great Meadows Ln
East Hanover NJ
Ph 973-887-9270
fax 973-887-3678
Gerry

> ----------
> From:         RSIMathis[SMTP:[log in to unmask]]
> Sent:         Tuesday, May 05, 1998 12:47 PM
> To:   [log in to unmask]
> Subject:      [TN] Uresolve Plus
>
> Hi, everyone.
>
> I'm looking for a chemical (solvent ?) called Uresolve or Uresolve Pls
> made by
> a company named Dynalloy. (I'm not sure about this name?)  This stuff
> is used
> for dissolving conformalcooatings and potting compounds.  Does anyone
> have any
> information where to purchase this substance OR how to contact this
> company?
> OR any info about a similar substance?
>
> What I'm trying to do is dissolve the plastic overmolding on a custom
> cable
> assembly to check out the internal construction.  I'm open to any and
> all
> suggestions.  Thanks for the help.
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe:   SUBSCRIBE TechNet <your full name>
> To unsubscribe:   SIGNOFF TechNet
> ################################################################
> Please visit IPC web site (http://jefry.ipc.org/forum.htm) for
> additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or
> 847-509-9700 ext.311
> ################################################################
>

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2