Yes, we've noticed that to. Why, we're not sure. But we changed the
material on our pallets and use a compressed fiberglass pallets. 
But the "frame" around our pallet is made of Al. There we can see solder
sticking pretty hard onto the frame. Strange.

/Jan Merstrand 

***************************************************************************