Morton has a full line of HI-TAC Panel Cleaners that are floor
models designed for cleaning panels in-line prior to
lamination of dry film as well as models designed for cleaning
laminated panels prior to exposing.
We do not have a cleaning unit designed to integrate into a
manual hot roll laminator.
Bob Stumpf, Morton Electronic Materials
>>> Scott <[log in to unmask]> 06/09/97 06:40pm >>>
Timothy,
Colight offers several models of what we call 'Film & Panel
Cleaners'.
Get in touch with me or your local Colight rep. for more info.
Regards,
-Scott
Timothy Gaylor wrote:
>
> Technet:
>
> I am looking for a tack roller machine to place before a hot
roll
> laminator to remove dust and debris from the panel. We
are havind
> problems with debris on panels before this process. If
anybody is aware
> of any product like this or have one to get rid of E-mail me
at Hound @
> webtv.net..
>
> Thanks,
>
> T.A. Gaylor
>
>
***************************************************************************
> * TechNet mail list is provided as a service by IPC using
SmartList v3.05 *
>
***************************************************************************
> * To subscribe/unsubscribe send a message <to:
[log in to unmask]> *
> * with <subject: subscribe/unsubscribe> and no text in the
body. *
>
***************************************************************************
> * If you are having a problem with the IPC TechNet forum
please contact *
> * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at
[log in to unmask] *
>
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using
SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to:
[log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the
body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum
please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at
[log in to unmask] *
***************************************************************************
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|