The Ionograph works by first dissolving the flux material, then measuring
those species that ionize. Small amounts of rosin will be tested with good
accuracy. However, if your parts have visible spots of rosin before (and
after) testing, then the test results will be both inaccurate and variable.
Unlike water soluble flux residues (which are very accurately tested in the
Ionograph), rosin does not dissolve well in IPA/water.
I would suggest letting the IPA/water warm as much as possible prior to
running a test, and run the first few tests on representative pieces for at
least 40 - 45 minutes to see if a plot of contamination vs time begins to
"flatten out". With the knowledge of how much contamination to expect,
you can then look to lower your test times to something more reasonable.
Apply your efforts here not to comply to traditional Mil Specs, but rather
to process control (hence alerting that a change has been introduced).
Greg Miller
L-3 Communications
Display Products
Alpharetta, GA 30004
770-346-8154
-----Original Message-----
From: Stolar, Paul W [mailto:[log in to unmask]]
Sent: Friday, May 02, 2003 2:50 PM
To: [log in to unmask]
Subject: [TN] Ionograph
Paul Stolar
Materials Engineer
Houston Technology Center
Baker Atlas
713-625-5376
713-625-4949 (fax)
It has been a while since I worked with rosin fluxes. How well does the
ionograph with IPA/H20 work?
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|