38G solid core? Sure, but you need to work harden it by bending it back and
forth. Also, if someone's iron runs hot, the wire dissolves into the solder
in about 10 secs, so it is easy to thin it below 4 mils without noticing.
38G nickel is much more robust if you're looking for something which stands
up to abuse.
Wayne
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Victor Hernandez
Sent: Friday, April 10, 2015 11:45 AM
To: [log in to unmask]
Subject: [TN] Copper wire open
Fellow TechNetters:
Is it possible for a 4 mil diameter copper wire open without any apparent
signs of elongation, mechanical stress? Can the copper wire snap cleaning
at the grain boundary?
Victor,
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|