Hi Technetters,
I'm interested in applying a test method for adhesion of layers in a multilayer.
I used to do a peel test and it worked fine with Teflon and even FR-4 layers
but Polyimide layers are just too
brittle to bend and peel. So instead I wish to do a "Lap shear test".
Can anybody help me out by pointing me to an applicable standard test method?
Thanks,
Yehuda
*************************************