Please be careful in making assumptions about G-10. There is nothing in any
specification that says that G-10 must burn so standard FR-4 meets all the
requirements.There was a time when some suppliers sold "FR-4/G-10" to make
this clear. Anyone who wishes to buy a laminate that contains no flame
retardents must ask specifically every time to be sure. And please don't
ask me because we do not make it in the UK.
***************************************************************************