Greetings,
Currently we are looking for a real-time x-ray inspection system for our
micro BGA & CSP assembly. The system should be able to allow us to rotate
the PCB at 360 degree for viewing solder joint quality (voids).
Furthemore, the system should equip with image processing - to measure the
percentage of solder voids.
So far I have only came across CRX-1000 from CR Technology (very brief).
Is anybody using this system before? Is so, how is its performance in
terms of images sharpness and magnification? In addition, can anyone
provide me its specification?
Since this is our first approach in selecting x-ray inspection equipment, I
also would like to ask if there is any aspects that I need to consider
before choosing the right one?
Many thanks in advance.
Cheers,
Daniel Woon
Manufacturing Engineer
[log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|