On 28 Aug 98 at 12:01, John Parsons wrote:
> Good Afternoon,
>
> We have received a board spec in German. The material call out is
> 6M15FR4I36K35
> We have interpreted this to mean:
>
> 6M - 6 layer
> 15 - 1.5mm overall thickness
> FR4 - FR4
> I36 - 0.36mm core (0.014")
> K35 - 35uCu (1oz Cu)
> Could someone please verify this?
That's right.
> Is this a standard euro spec (if so whose, and how do I get more information
> on it) or just this companies internal spec.
I might be an ILFA spec. I don't know whether it's standard, You
can find a description what this ILFA syntax means (in german....) under their URL
http://www.ilfa.de/ilfa/dokumente/multilayer_bautypen/syntax_fuer_bautypen_bezeichnungen.html
and I will mail as attachment with this mail directly to you (not to the listserver!) their PDF
file (10kB) with the drawing of 6M15FR4I36K35.
Hope this helps
Regards
Matthias Mansfeld
-----------------------------------------------
Matthias Mansfeld Elektronik
* Printed Circuit Board Design and Assembly
Am Langhoelzl 11, D-85540 Haar, GERMANY
Phone: +49-89-4620 0937, Fax: +49-89-4620 0938
E-Mail: [log in to unmask]
Internet: http://home.t-online.de/home/matthias.mansfeld
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|