Hello Emily,
I've always thought it meant Room Temperature Vulcanising.
Phil.
-----Original Message-----
From: Emily Tse [mailto:[log in to unmask]]
Sent: Friday, 23 March 2001 14:29
To: [log in to unmask]
Subject: Re: [TN] FW: [TN] Solvent for RTV738
sorry all, mind to explain what's RTV stand for?
------Original Message------
From: Bev Christian <[log in to unmask]>
To: [log in to unmask]
Sent: March 22, 2001 4:49:32 PM GMT
Subject: [TN] FW: [TN] Solvent for RTV738
Below is a message from Jeff Geraden that I thought I should share with all
of you.
Is it your collective opinion that I should now eat my shorts? :) Now I
want to know HOW this stuff works, even though I don't need to dissolve any
silicones right now.
Bev Christian
Research in Motion
-----Original Message-----
From: Gerarden, Jeff [mailto:[log in to unmask]]
Sent: March 22, 2001 11:36 AM
To: 'Bev Christian'
Subject: RE: [TN] Solvent for RTV738
Bev,
This material I know will dissolve Dow Corning 3145 from previous
experience. I am confident it will on other cured silicone RTV's. I forgot
to specify cured or uncured. I used the Dynasolve 225 and did not use any
other dynasolve choices. Make sure you obtain a Technical Data Sheet before
use. Some very important/good information on it.
http://www.dynaloy.com/dynasolve200series.htm
>
>
> Jeff Gerarden
> Focus Factory Supervisor
> PLEXUS-ELECTRONIC ASSEMBLY CORP.
> 2121 Harrison St. Neenah WI 54956
> phone: (920) 751-3226
> email: [log in to unmask]
> http://www.plexus.com
>
>
> -----Original Message-----
> From: Bev Christian [SMTP:[log in to unmask]]
> Sent: Thursday, March 22, 2001 7:16 AM
> To: 'TechNet E-Mail Forum.'; 'Gerarden, Jeff'
> Subject: RE: [TN] Solvent for RTV738
>
> Jeff,
> 1) I tried Dynasolve.com and was not taken to their web page.
> 2) Are you saying that this stuff will dissolve cured or uncured
> silicones?!
>
> Bev Christian
> Research in Motion
>
> -----Original Message-----
> From: Gerarden, Jeff [mailto:[log in to unmask]]
> Sent: March 22, 2001 2:57 AM
> To: [log in to unmask]
> Subject: Re: [TN] Solvent for RTV738
>
>
> If this material is a silicone I have used Dynasolve 225 to dissolve the
> Dow
> Corning RTV on several PCB's with great success. You could find the
> company
> on the web by typing the product name above. Make sure you look at the
> technical data sheet on this material. Hope this helps you out.
>
> > Jeff Gerarden
> > Focus Factory Supervisor
> > PLEXUS-ELECTRONIC ASSEMBLY CORP.
> > 2121 Harrison St. Neenah WI 54956
> > phone: (920) 751-3226
> > email: [log in to unmask]
> > http://www.plexus.com
> >
> >
> > -----Original Message-----
> > From: <Peter George Duncan> [SMTP:[log in to unmask]]
> > Sent: Tuesday, March 20, 2001 8:12 PM
> > To: [log in to unmask]
> > Subject: [TN] Solvent for RTV738
> >
> > Hi, TechNetters,
> >
> > I am trying to find a solvent for removing 3M's RTV 738 that has been
> used
> > for bonding components to a number of boards, or to each other. Any
> > suggestions?
> >
> > I have tried 3M themselves and they have no solvent of their own apart
> > from
> > "Citrus Base Adhesive Remover" that 'may soften' it enough to peel it
> off,
> > but this seems pretty indefinite.
> >
> > Thanks in hope
> >
> > Pete Duncan
> > Asst Principal Engineer
> > Singapore Technologies Aerospace
> >
> >
> --------------------------------------------------------------------------
> > -------
> > Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> > To unsubscribe, send a message to [log in to unmask] with following text
> in
> > the BODY (NOT the subject field): SIGNOFF Technet
> > To temporarily halt delivery of Technet send the following message: SET
> > Technet NOMAIL
> > Search previous postings at: www.ipc.org > On-Line Resources & Databases
> >
> > E-mail Archives
> > Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> > additional
> > information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> > ext.5315
> >
> --------------------------------------------------------------------------
> > -------
>
> --------------------------------------------------------------------------
> --
> -----
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET
> Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
> E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> --------------------------------------------------------------------------
> --
> -----
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
______________________________________________
FREE Personalized Email at Mail.com
Sign up at http://www.mail.com/?sr=signup
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|