http://www.binghamton.edu/physics/cottsectc.pdf
Here is the link to the study, sorry.
Dave C.
-----Original Message-----
From: Eric Dawson [mailto:[log in to unmask]]
Sent: Wednesday, June 04, 2003 9:53 AM
To: [log in to unmask]
Subject: Re: [TN] BGA problems on ENIG
Dave,
Do you have a reference so we can read the paper/study please?
Regards
Eric Dawson
> -----Original Message-----
> From: Dave Chapman [SMTP:[log in to unmask]]
> Sent: Wednesday, June 04, 2003 3:39 PM
> To: [log in to unmask]
> Subject: Re: [TN] BGA problems on ENIG
>
> Hi, just got e-mail from board supplier warning of tendency of BGA
breaking
> off ENIG pads. Citing a study at University of NY at Binghamton from a few
> years ago. Claim growth of (Au0.5Ni0.5) at the Ni3Sn4/solder interface
> promoting brittle joints. Board house was using HASL and we prefer
Immersion
> Silver but hadn't heard of the ENIG problem with BGA's
> Any comments?
> Dave Chapman
> Manufacturing Engineer
> Circuit Service Inc.
>
>
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|