<< Is conformal coating a good protection against dendrites? >>
Graham's answer is a very good one. In a way, this question reminds me of an
advertisement that I often saw in bicycling magazines during my college days.
It was for a new type of lock to hold one's bicycle to the parking rack, and
it had for a headline "Resists Atomic Bombs". The key being that it was not
100% successful, but it did offer resistance.
In every comparative test that I have ever done, uncoated boards fared far
worse than coated ones with respect to dendritic growth. Does that mean that
conformal coating will prevent dendrites from EVER appearing? Clearly not.
My typical tests were 100 hours at 85 C and 85% RH, with power applied, with
the acrylic coated boards normally surviving the entire test and the uncoated
boards failing in 2-8 hours, depending on the soldering process variables
involved.
Jon Moore
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|