isola USA
100 Tillessen Blvd.
Ridgeway, SC 29130
+1-803-337-4000
+1-803-337-8821 fax
20 July 1998
To: Isola USA Customers
Subject: Conversion to IPC-4101 from MIL-S-13949H
As of 30 November 1998, MIL-S-13949H will be canceled by the Defense
Supply Center Columbus (DSCC). This means that all references to
MIL-S-13949 must be removed from labels, certificates of compliance,
part numbers and other pertinent drawings relative to base materials and
printed boards. At that time isola USA will only issue certificates of
compliance for IPC-4101 which was published December 1997 by the IPC.
Isola USA will not be able to certify any base materials to MIL-S-13949H
after the 30th November date.
Our understanding of the DSCC policy is the 30 November 1998 timeline is
on a "point of sale" basis. Materials manufactured before this date but
certified after 30 November will still only carry the IPC-4101
certification. Materials shipped from distribution warehouses after
30th November 1998 will have the MIL-S-13949H reference, the Cage Code
and the Qualification Reference Number (QRN) crossed off and IPC-4101
inserted on certificates of compliance and master box labels.
From a customer viewpoint, the quality levels of base materials shipped
will not be affected by this certification change since the performance
requirements of IPC-4101 are equal to or more stringent than
MIL-S-13949H. Isola USA still plans to conduct what is the equivalent
of Group A, B and C inspection on laminates and prepregs as directed by
IPC-4101 and our Quality Management Team (QMT). All new product grades
not previously listed on a MIL-S-13949H Qualified Product List (QPL)
will be qualified at an independent test laboratory and the data readily
available for review.
I have attached a summary of some of the differences between the two
specifications as well as a template letter for you to use with your
customers. If you have any questions concerning IPC-4101, please call
me directly at 803-337-4203 or fax me your questions at 803-337-8821.
With kind regards,
Douglas J. Sober
Corporate Director of Quality
SIGNIFICANT DIFFERENCES BETWEEN
MIL-S-13949H AND IPC-4101
General Information Differences
Prepregs and laminates are on the same slash sheet.
Slash sheets are organized by "families" with open spaces for new
materials that fit the family concept.
The entire specification is in metric with no English references.
The latest test methods are attached to the document.
Paragraph 1.2.2
Laminates can be ordered as a dielectric space (without copper) or as an
overall thickness (including copper) foil. Currently laminates can only
be ordered as a dielectric space.
Table 1
The copper foil table now includes type "R", reverse treated
electrodeposited for grade 1 and type "S" for reverse treated
electrodeposited for grade 3.
Paragraph 1.2.5 and 3.8.3.1.2
Surface Quality Class now includes a "D" designation which provides the
most stringent surface quality call-out. No pits, dents or epoxy spots
over 5 mils. MIL-S-13949H has "B" as the tightest class which allows 1
pit up to 15 mils.
Paragraph 1.2.7
Prepregs are ordered using 3 parameters, resin content, resin flow, and
the "optional" parameter. Prepreg can be tested by new test methods
such as rheology, % Cure, or delta.
Paragraph 3.1.2
Quality Conformance Testing is conducted as determined by the
Manufacturers Quality System as outlined in IPC-PC-90. In the absence
of a Manufacturing Quality System, conformance testing is conducted at
the same frequency as MIL-S-13949H.
Paragraph 3.1.5, and 3.3
Self declaration form IPC-LQP-1730 is a prerequisite to certifying to
IPC-4101. The document IPC-LQP-1730 will be published by the IPC at the
same time as the IPC-4101 specification.
Paragraph 3.1.7 and 3.4
Qualification testing must be conducted by the supplier at any
IPC-QL-653 approved laboratory. The qualification data must be
summarized and readily available for review. The qualification testing
regime is the same as prescribed by MIL-S-13949H.
Paragraph 3.4.1
A thin laminates specimen 10 mils or less qualifies all thin laminates
(30 mils and less). A thick laminate specimen greater than 30 mils
qualifies all thick laminates.
Paragraph 3.4.2
For a given slash sheet, the thinnest prepreg qualifies all the thicker
prepregs.
Table 5
Table 5 now includes Delta Tg and Average X/Y CTE as optional tests.
In the absence of a Manufacturers Quality System, the frequency of
testing is the same as MIL-S-13949H.
The test method for flammability has been changed from the "MIL" method
to the standard UL method 94.
Table 6
Electrical tests and some environmental tests are performed on prepregs
after pressing into a thin laminate.
Prepreg testing for flammability is only conducted as a thin laminate
specimen.
Paragraph 3.9.1.1
Peel Strength is called out as a single value for 35 micron foil. Foil
weights greater than 35 micron must meet the required value for 35
micron. Foils less than 35 micron may be plated up to 35 micron and
tested as is the current specified procedure in MIL-S-13949H.
Paragraph 3.9.1.2
Dimensional stability is now specified as a nominal value with a
tolerance range. The supplier must provide the nominal value for
dimensional stability for each construction. Currently the MIL-S-13949H
specification uses zero as the nominal value. IPC-4101 will reward
consistency of dimensional movement.
Paragraph 3.9.2.2.6
Gel Time is an optional test. It can be replaced with other
characterization tests if desired such as rheological flow, Cure % or
Delta H.
Paragraph 3.9.2.2.8
Volatile Content is an optional test.
Paragraph 3.10.2.3
Dicy Crystals is an optional test.
Paragraph 3.15
MSDS forms must be available for materials supplied under this
specification.
Paragraph 5.2
The supplier is responsible for establishing written guidelines for
their authorized distributors.
Template Letter
(To be used by the printed circuit shop to their customer)
(Name of the contact at your Customer)
(Your Customer's name)
(Your Customer's business address)
Dear …….,
As you may be aware, MIL-S-13949H and its associated Qualified Product
List (QPL) will be canceled as of 30 November 1998. The Defense Supply
Center Columbus (DSCC) communicated the cancellation in a letter from
David M. Moore dated 11 June 1998. By definition from the personnel at
DSCC, cancellation means that (your name) will not be able to purchase
laminates and prepregs certified to MIL-S-13949H any longer. Our
current suppliers of base materials have informed (your name) that
certificates of compliance and related paperwork will only reflect
IPC-4101, a base materials specification developed by industry experts
within the IPC and published in December 1997 after the cancellation
date.
From our viewpoint, the quality levels of base materials received by
(your name) and shipped to (your Customer's name) will not be effected
by this certification change as the requirements of IPC-4101 are equal
to or more stringent than MIL-S-13949H.
In preparation for this change, (your name) would like the purchasing
information and drawings of (your Customer's name) to now reflect
certification to IPC-4101 in place of MIL-S-13949H. At the very least
we request a letter from (your Customer's name) indicating that you
accept the IPC-4101 replacement of MIL-S-13949H for certification
purposes.
The conversion to IPC-4101 is a few short months away. We need to start
working together now to prevent confusion on 30 November 1998.
Please contact me at your earliest convenience at (your telephone
number).
Sincerely yours,
(your name)
(your title)
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|