Inge, you bring back all the memory too. One of the wood shipping box got stolen at trade show at my prior jig place. Thx God the demo piece inside was made by home designed robot. Hard to reverse engineering. But it was still a very upset event for all engineer team. No Russian, but possibly went to some warm places. :-(. Did you see Samsung lost 2 OLED TV at trade show in EU recently? Wood display piece is a billion move for sure. I wish we did put pop corn in that wood box only.
--------------------------
Sent using BlackBerry
From: Inge Hernefjord [mailto:[log in to unmask]]
Sent: Tuesday, December 11, 2012 05:36 PM
To: TechNet E-Mail Forum <[log in to unmask]>; Joyce Koo
Subject: Re: [TN] Polymer Lid
When you say that, Joyce, I remember a practical joke we played 30 years ago. We were pretty good at so called 'hybrids', RF type, ceramic substrates mounted in machined Kovar packages. We made a couple of packages of wood and sent them to an expo in USA. On the stand's wall you could read that this was a way to lower the costs essentially. Caused many smiles and also serious questions. They were stolen last day, and we chuckled " russians". This was in the days humor was larger part of the daily work than it is today.
Inge
On 11 December 2012 15:19, Joyce Koo <[log in to unmask]<mailto:[log in to unmask]>> wrote:
Why not metal lid? With such a low volume, can't be the cost.
--------------------------
Sent using BlackBerry
----- Original Message -----
From: Steven Creswick [mailto:[log in to unmask]<mailto:[log in to unmask]>]
Sent: Tuesday, December 11, 2012 08:44 AM
To: [log in to unmask]<mailto:[log in to unmask]> <[log in to unmask]<mailto:[log in to unmask]>>
Subject: Re: [TN] Polymer Lid
Ken,
I did not mean to imply that this would create a seal to keep moisture out,
but simply to point out that an enclosed volume of gas will expand when
heated. If one is not prepared for this, it can cause surprises.
We did things like this in the hybrid industry over 30 years ago, using
ceramic substrates and ceramic shells/lids. Definitely NOT hermetic, but
served their purpose for industrial applications.
I believe that Zytel is a glass reinforced polyamide. Not familiar with
this particular one, but my experience with LCP's has been that they can
offer greater temperature resistance, but likely cost more....
Try it before you buy it! Get some samples from the folks cited.
Steve Creswick
Sr Associate - Balanced Enterprise Solutions
http://www.linkedin.com/in/stevencreswick
616 834 1883<tel:616%20834%201883>
-----Original Message-----
From: Kenneth J. Wood [mailto:[log in to unmask]<mailto:[log in to unmask]>]
Sent: Tuesday, December 11, 2012 8:19 AM
To: 'TechNet E-Mail Forum'; 'Steven Creswick'
Subject: RE: [TN] Polymer Lid
The units are not airtight and some small amount of moisture is inevitable /
acceptable.
The linx guys got back to me and said that they use Zytel HTNFR52G30
Polyimide for thier lids.
Any thoughts?
Ken
-----Original Message-----
From: TechNet [mailto:[log in to unmask]<mailto:[log in to unmask]>] On Behalf Of Steven Creswick
Sent: Monday, December 10, 2012 7:20 PM
To: [log in to unmask]<mailto:[log in to unmask]>
Subject: Re: [TN] Polymer Lid
Ken,
Also consider that if you seek to create an enclosed cavity, the air inside
that cavity will expand during heating and sometimes create blow holes in
the 'seal' during heat cure of the adhesive. Similarly, during reflow,
depending upon the adhesive used, you can 'pop' the lids off.
I've encountered situations in the past where a small hole was left in the
lid to avoid the 'over pressurization scenario' and then 'sealed'
post-reflow.
Can you use a deep drawn metal lid as opposed to a folded type metal
lid/shield?
You could use a logo on sticker to cover the vent hole afterwards...
Steve Creswick
Sr Associate - Balanced Enterprise Solutions
http://www.linkedin.com/in/stevencreswick
616 834 1883<tel:616%20834%201883>
-----Original Message-----
From: TechNet [mailto:[log in to unmask]<mailto:[log in to unmask]>] On Behalf Of Kenneth J. Wood
Sent: Monday, December 10, 2012 6:58 PM
To: [log in to unmask]<mailto:[log in to unmask]>
Subject: Re: [TN] Polymer Lid
Bob,
I'm using a metal lid for the larger size modules now and it is a pain to
say the least to solder them on manually.
One of the issues in the past was liquids getting under the lid during
cleaning.
That's why I wanted a plastic lid with no seams that could be filled with
goo and glued down.
These units are supplied as a module to end uses so they have to have the
lids on from us.
Ken
-----Original Message-----
From: Robert Kondner [mailto:[log in to unmask]<mailto:[log in to unmask]>]
Sent: Monday, December 10, 2012 6:48 PM
To: 'TechNet E-Mail Forum'; 'Kenneth J. Wood'
Subject: RE: [TN] Polymer Lid
Kenneth,
Yes, I looked at your link so now I see better. Your users will be doing a
reflow.
So you need a thermoset lid. Glue it on with a silicon and I think you are
set except maybe for cleaning.
I would imagine your customer will clean their boards which would tend to
trap fluids under the lids. So then you get into the area of filling and
sealing? That is a mess. It gets worse as you have SMT leads coming off the
PCB. If you can place filling holes in the PCB you can get the right amount
of material in the unit except for the filling of voids. I played with this
once and using a vacuum fixture to removed voids can cause a mess. You need
to vacuum then fill with the vacuum applied. Then reintroducing air fills
voids as air pushed down through the fill holes.
A mess to fixture.
You might look at cavist.com<http://cavist.com/> as they do low temp thermoplastics, maybe they
can do a low temp thermoset so you can encapsulate soldered modules.
Or consider metal cans? :-)
Getting the right amount of fill material to provide a filled sealed device
is very difficult.
Bob K.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]<mailto:[log in to unmask]>] On Behalf Of Kenneth J. Wood
Sent: Monday, December 10, 2012 6:04 PM
To: [log in to unmask]<mailto:[log in to unmask]>
Subject: Re: [TN] Polymer Lid
Bob,
Thanks for your help on this.
Quantities are 1,000 to 50,000 per year and the lid needs to be glued on
before it ships to the end users.
Ken
-----Original Message-----
From: TechNet [mailto:[log in to unmask]<mailto:[log in to unmask]>] On Behalf Of Robert Kondner
Sent: Monday, December 10, 2012 5:58 PM
To: [log in to unmask]<mailto:[log in to unmask]>
Subject: Re: [TN] Polymer Lid
Kenneth,
I looked into this some years back and any material that "Stands Up" to
reflow temps would be difficult to form. Injection molding would probably be
impossible but ask, don't take my word.
At all costs is there any way to add it as a last step addition to a
finished PCB?
How many are you talking about?
I did have some plastic parts made from a thermoset. It was black material
and I forgot the trade name. It was probably just a phenolic material. Not
sure how well it takes reflow temps. If you need help contact me off line, I
will get you a sample. I had some 2 x 4 inch boxes and cover made.
Bob K.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]<mailto:[log in to unmask]>] On Behalf Of Kenneth J. Wood
Sent: Monday, December 10, 2012 5:30 PM
To: [log in to unmask]<mailto:[log in to unmask]>
Subject: [TN] Polymer Lid
Hi all,
I need to design a polymer lid that gets glued on top of a square PCB.
The lid will be 0.66" x 0.66" by 0.20" (maybe 0.025" wall thickness) with a
flat top so I can have the company logo and part number printed on it.
The PCB itself is a system that gets soldered to a main board by way of
castellated holes.
My question is, what lid material should I use since this unit must go
through a reflow over?
I assume a vacuum formed CPVC lid would melt right?
The unit is somewhat similar in mechanical characteristics to a Linx module
like the TXM-xxx-es
https://www.linxtechnologies.com/resources/data-guides/txm-xxx-es.pdf
Thanks
Ken
_____________________________________
Kenneth J. Wood
Saturn PCB Design, Inc.
[log in to unmask]<mailto:[log in to unmask]>
www.saturnpcb.com<http://www.saturnpcb.com/>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]<mailto:[log in to unmask]>
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]<mailto:[log in to unmask]>
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]<mailto:[log in to unmask]>
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]<mailto:[log in to unmask]>
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]<mailto:[log in to unmask]>
______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]<mailto:[log in to unmask]>
______________________________________________________________________
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]<mailto:[log in to unmask]>
______________________________________________________________________
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|