I have been involved with ENIG failures since '98. The quality of the ENIG
chemistry has improved tremendously since then, but I continue to move
customers from ENIG to other alternatives. Most of this is caused by black
pad. The problem is that black pad often requires months to develop and I
have not found a reliable test to be used immediately after fabrication to
predict whether on not the coating will be black pad prone. Consequently, I
am very uncomfortable with ENIG.
Best regards
Lee
J. Lee Parker, Ph.D.
JLP Consultants LLC
804 779 3389
----- Original Message -----
From: "Steve Kelly" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Friday, June 29, 2007 10:42 AM
Subject: [TN]
> Good Morning to All,
>
> I have a customer who has asked me to do an on-going test for black pad.
> The
> test would require me to solder wires onto 624 BGA pads and then pull on
> the
> wires to determine if there is black pad . They have given me no criteria
> in
> terms of pull strength or what constitutes pass/fail. I obviously need
> some
> kind of pull tester to do this. Has anyone done anything similar? Any
> thoughts or ideas would be appreciated. Regards Steve Kelly
>
>
>
> Steve Kelly
>
> (416) 750-8433 (work)
>
> (416) 750-0016 (fax)
>
> (416) 577-8433 (cell)
>
>
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|