Kelly,
During our investigation into electroless nickel/immersion gold for military
PWB's, I did not find any military specifications for immersion gold. I could
only find IPC specs for immersion gold.
We settled on three tests to verify the proper gold plating. They were
thickness using x-ray flourescence, adhesion of the gold per MIL-P-55110D,
(Amendment 1) and solderability per MIL-P-55110D (Amendment 1).
Good Luck!
Tom
_______________________________________________________________________________
From: Baker,Kelly on Wed, Apr 9, 1997 3:38 PM
Subject: specifications
To: [log in to unmask]
Hi!
Does anyone know of any Military of non Military specs for immersion
gold? We know of the IPC-6012. Any information would be appreciated.
Thanks,
Kelly
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
------------------ RFC822 Header Follows ------------------
Received: by msgw.vf.lmco.com with ADMIN;9 Apr 1997 15:37:53 -0400
Received: from dekalb.vf.mmc.com (dekalb.vf.mmc.com [192.35.35.21]) by
franklin.vf.lmco.com (8.7.6/8.7.3) with ESMTP id PAA00224; Wed, 9 Apr 1997
15:37:12 -0400 (EDT)
Received: from simon.ipc.org ([168.113.24.64]) by dekalb.vf.mmc.com
(8.7.6/8.7.3) with SMTP id PAA04492; Wed, 9 Apr 1997 15:37:10 -0400 (EDT)
Received: from ipc.org by simon.ipc.org via SMTP (940816.SGI.8.6.9/940406.SGI)
id OAA20273; Wed, 9 Apr 1997 14:25:10 -0700
Resent-Date: Wed, 9 Apr 1997 14:25:10 -0700
Received: by ipc.org (Smail3.1.28.1 #2)
id m0wF1zs-000BkGC; Wed, 9 Apr 97 13:21 CDT
Resent-Sender: [log in to unmask]
Old-Return-Path: <[log in to unmask]>
Message-ID: <[log in to unmask]>
From: "Baker,Kelly" <[log in to unmask]>
To: "[log in to unmask]" <[log in to unmask]>
Subject: specifications
Date: Wed, 9 Apr 1997 14:33:24 -0400
X-Mailer: Microsoft Exchange Server Internet Mail Connector Version 4.0.837.3
MIME-Version: 1.0
Content-Type: text/plain; charset="us-ascii"
Content-Transfer-Encoding: 7bit
Resent-Message-ID: <"zTR_u2.0.DZA.NuzIp"@ipc>
Resent-From: [log in to unmask]
X-Mailing-List: <[log in to unmask]> archive/latest/11814
X-Loop: [log in to unmask]
Precedence: list
Resent-Sender: [log in to unmask]
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|