TECHNET Archives

1996

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Scott B. Westheimer" <[log in to unmask]>
Date:
Wed, 18 Sep 1996 18:30:49 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (27 lines)
From: Scott Westheimer
Date: 9/17/96

Sorry if my message of last night was not very clear, but what can you
expect at 2:30 am. 

The issue is with entek coating not the gold plating. The panels have
selective gold plating on some pads and the others have entek. The problem
is that when the panels are first gold plated( electrolydicly ), then S/M 
the entek pads are fine. However, when the panels are first S/M and then
gold plated the entek pads are tarnished around the edges. Does anyone have
experience with this problem.

Thanks,

PS Before anyone makes the comment, the boards are enticed after all the
processes have been completed.

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



ATOM RSS1 RSS2