Frank,
Did you use a "Glue/Paste" process on the SMT that is on the Wave side, or,
did you get those nice fillets from the wave?
IF you got them from the wave, the questions become:
1. Why nice wetting on the SMT and not on the TH pads?
2. How was the bare board processed at the Fab level?
Before looking at the photos I thought the leads of the comps were contaminated,
or, the profile was insufficient, or, your contact angle and dwell times were
not quite sufficient. But, after looking at the photos and seeing the nice
topside fillet on the TH and nice SMT fillets, I get the feeling that the
plating on the bottomside of the board at the TH comps was compromised at the
fab level. Maybe the resist was not sufficiently removed prior to plating.
It's hard to tell from the photo, but, where there is insufficient wetting on
the wave side pad, what does that section look like? What color is it?
-Carrie
-----Original Message-----
From: Frank L Norman [mailto:[log in to unmask]]
Sent: Monday, July 28, 2003 1:26 PM
To: [log in to unmask]
Subject: [TN] Wave solder process issue on ENIG pwa
Technet,
Looking for comments for the following...
PWA's experienced solder wetting difficulties to plated through holes
including via's during the wave solder process and are unable to be
touched-up by hand. PWA's are two sided multilayer with combination of
rigid board and flex circuits finished with Electroless Nickel Immersion
Gold (ENIG) for a thickness of 100 microinches of Nickel and 5 microinches
of Gold. Top side SMT components were reflowed and bottom side SMT were
wave soldered with excellent results, but as you can see in the pictures
the plated through holes on the wave soldered side had wetting issues.
Interesting thing is the non wave solder side through holes have good
wetting.
SEE PICTURES of pwa's in question at this website.
http://www.ripus.com/images/pwa/index.htm
Regards,
Frank Norman
Manufacturing Support Engineer
Raytheon, Space and Airborne Systems (SAS)
(805)879-2745
[log in to unmask]
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|