Hi Inge!
I have done thick film gold etching--the results are easy and very
pretty. Spin on positive photo-resist. Very good results with co-fired
gold on LTCC because shrinkage minimizes voids. DuPont had or has a few
decent products for this: Fodel, 5771, and the cofired LTCC stuff.
Etchant is potassium iodide. Turns everything yellow--almost as bad as
FeCl. We were able to achieve 1mil lines with 1.5 mil space, but was a
real pain since AOI can't inspect that level of detail very well and
standard photoplots are at the limits of their resolution.
Wayne
>>> [log in to unmask] >>>
Hi, anyone happen to have this report?
THIN PRINT ETCHABLE GOLD-AN ALTERNATIVE TO THICK AND THIN FILM
HSU, K.F.
08 Oct 1986
ADVANCED MICRODEVICES
Inge
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|