Phil,
I've no direct experience of failures definitely attributed to
ultrasonic cleaning, but I'd refer you to 'Reliability and Yield
problems of Wirebonding in Microelectronics' Harman, G.
ISBN: 0-930815-25-4 available from ISHM.
There is a discussion on this issue, in the book, with references.
>From my perspective, dealing with PEMs, the key message is that
cleaning frequencies >100kHz are unlikely to cause any damage.
regards
Olly
> From [log in to unmask] Fri Jun 6 19:24:55 1997
> Resent-Date: Fri, 6 Jun 1997 14:23:14 -0400 (EDT)
> Resent-Sender: [log in to unmask]
> Old-Return-Path: <[log in to unmask]>
> From: [log in to unmask]
> Date: Fri, 6 Jun 1997 14:23:14 -0400 (EDT)
> To: [log in to unmask]
> Subject: Ultrasonic Cleaning
> Resent-Message-Id: <"xyI872.0.4lO.mC5cp"@ipc>
> Resent-From: [log in to unmask]
> X-Mailing-List: <[log in to unmask]> archive/latest/13215
> X-Loop: [log in to unmask]
> Resent-Sender: [log in to unmask]
> Content-Length: 1197
>
> I have a argument going on ultrasonic cleaning of PWA's with different types
> of component.
>
> Several opinions have come up:
> (1) Never ultrasonic clean if you have hybrids with wire bond connections.
> (2) Hybrids are OK to clean in an ultrasonic if an encapsulant is used.
> (3) Hybrids are OK to clean if they supplier follows standard wire bond
> requirements.
> (4) Do any of the above rules apply to multichip modules.
> (5) Do Ball Grid Array fall in any of the above categorties.
>
> Phil Hinton
> [log in to unmask]
>
> ***************************************************************************
> * TechNet mail list is provided as a service by IPC using SmartList v3.05 *
> ***************************************************************************
> * To subscribe/unsubscribe send a message <to: [log in to unmask]> *
> * with <subject: subscribe/unsubscribe> and no text in the body. *
> ***************************************************************************
> * If you are having a problem with the IPC TechNet forum please contact *
> * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
> ***************************************************************************
>
>
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|