We have been using Enthone DSR-3241 for 6 years now and have never UV
bumped the soldermask after thermal cure. We do not have a solder
ball problem using this soldermask and our non-UV bump process.
How big are your balls, how many do you have, and when do you see
them?
______________________________ Reply Separator _________________________________
Subject: Solder Balls
Author: [log in to unmask] at corp
Date: 2/7/96 2:56 PM
Has anyone experienced solder balls with the elimination of
UV bump after thermal cure and specifically with Enthone mask?
How does one go about solving the solder balls problem?