Steve,
Judging by the picture, it appears that the ENIG plating is missing from
those pads. If you take a pink pearl eraser, and lightly rub those pads,
they should turn copper in color. You may have issues when trying to
solder to those pads.
Ron
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Tuesday, April 29, 2008 10:19 AM
To: [log in to unmask]
Subject: [TN] ENIG PCB Problem...
Hi All!
We just got some boards in this morning that we were supposed to be
building on a quick turn. The lot was supposed to be 25 assemblies, but
we only got 11 boards.
We noticed something at a few pads of a device footprint that looked
pretty bad. Check out:
http://stevezeva.homestead.com/Dark_Pads.jpg
http://stevezeva.homestead.com/Dark_Pads_Close.jpg
If it isn't obvious, the boards are ENIG. These pads stood out right
away with the naked eye, and when we started looking closely at the
boards, we noticed other dark looking pads, but not nearly as bad as
what you see in the photo.
If I've been paying attention correctly, I can't call this black pad.
Black pad needs more than just a visual indication such as this, right?
We looked at all 11 boards, but only found 4 of them with any problems.
Only one of four had the problem as bad as what is in the photo.
My feeling is that we shouldn't run any of them, no matter if we can see
a problem or not...
Of course we're getting in touch with our fab house about this, but we
haven't heard back from them yet. This just happened a couple of hours
ago.
Thanks!
Steve
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|