Richard,
If you mean the best resistance to UV weathering (colour change, embrittlement), then silicone chemistries are probably better than acrylics or epoxies. Get something which fully cross-links.
Regards,
Peter
Peter Swanson
Managing Director
INTERTRONICS
Oxfordshire, England
t +44 1865 842842
e [log in to unmask]
www.intertronics.co.uk
INTERTRONICS is the trading name of Cygnet Electronics Ltd, registered in England No 1835617
Registered office: 12a Station Field Industrial Estate, KIDLINGTON, Oxfordshire, OX5 1JD, ENGLAND
INTERTRONICS is certified to ISO 9001:2015
-----Original Message-----
From: TechNet <[log in to unmask]> On Behalf Of Richard Kraszewski
Sent: 10 February 2021 16:10
To: [log in to unmask]
Subject: [TN] Most UV Resistant (conformal) coating?
Anyone have a clue as to what type of coating that would be?
Rich Kraszewski
Plexus Senior Staff Process Engineer
* * * * * * * * CONFIDENTIALITY NOTICE * * * * * * * * This e-mail and any attachments are confidential from Plexus Corp. and may contain information which is privileged, confidential, and/or protected by non-disclosure agreements. They are intended solely for the use of the named addressee(s). . Any unauthorized use or disclosure may be unlawful. If you are not a named addressee, you must not use, disclose, retain or reproduce all or any part of the information contained in this e-mail or any attachments If you have received this transmission in error, please destroy it and notify us immediately by return e-mail or by calling + 1 888 208 9005.
|
|
|