Good Day to everyone,
We have been experiencing an issue with deep gold plating after etch. The
undercut is breaking away making the traces look "hairy." The gold either
clings and drags away from the trace or breaks loose at LPI/Soldermask and
floats in the ink to some other undesireable location. It is not consistent
but it is persistant. Has anyone had this issue before and could someone
suggest some possible solutions? (It never happens with standard copper
plating--just deep gold.)
Thanks,
Steve MacDonald
Mass Design
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------